CCS Grade shipbuilding steel plate

[!--oldtitle--]

CCS Grade shipbuilding steel plate

EN 10025-2 is European standard, EN 10025-2 Carbon Steel is a steel alloy where carbon is the main alloying element.

Carbon steel can be grouped into 3 categories: Low Carbon Steel (also known as Mild Steel), Medium Carbon Steel and High Carbon Steel.

  • Keywords: CCS shipbuilding plate grade
  • Pageviews:

CCS shipbuilding plate grade AQ DQ EQ FQ AH EH FH 36 40 47 51 63 70 chemical and mechanical properties

CCS Shipbuilding Plate Product introduction:

CCS Grade FQ70 Shipbuilding Steel Plate:

C max

Si max

Mn

P max

S max

N max.

0.18

0.55

1.60

0.020

0.020

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

690

770-940

14

CCS Grade EQ70 Shipbuilding Steel Plate:

C max

Si max

Mn

P max

S max

N max.

0.20

0.55

1.70

0.025

0.025

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

690

770-940

14

CCS Grade DQ70 Shipbuilding Steel Plate:

C max

Si max

Mn

P max

S max

N max.

0.21

0.55

1.70

0.035

0.035

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

690

770-940

14--16

CCS Grade AQ70 Shipbuilding Steel Plate:

C max

Si max

Mn

P max

S max

N max.

0.21

0.55

1.70

0.030

0.030

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

690

770-940

14

CCS Grade EQ63 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.20

0.55

1.70

0.025

0.025

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

620

720-890

15

CCS Grade FQ63 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.18

0.55

1.60

0.020

0.020

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

620

720-890

15

CCS Grade AQ63 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.21

0.55

1.70

0.030

0.030

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

620

720-890

15

CCS Grade EQ56 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.20

0.55

1.70

0.025

0.025

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

550

670-830

16

CCS Grade FQ56 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.18

0.55

1.60

0.020

0.020

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

550

670-830

16

CCS Grade AQ56 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.21

0.55

1.60

0.030

0.030

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

550

670-830

16

CCS Grade EQ51 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.20

0.55

1.70

0.025

0.025

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

500

610-770

16

CCS Grade FQ51 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.18

0.55

1.60

0.020

0.020

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

500

610-770

16

CCS Grade AQ51 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.21

0.55

1.70

0.030

0.030

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

500

610-770

16

CCS Grade EQ47 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.20

0.55

1.70

0.025

0.025

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

460

570-720

17

CCS Grade FQ47 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.18

0.55

1.60

0.020

0.020

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

460

570-720

17

CCS Grade AQ47 Shipbuilding Steel Plate

C max

Si max

Mn

P max

S max

N max.

0.21

0.55

1.70

0.030

0.030

0.020

Yield Strength (MPa) min.

Tensile Strength (MPa)

Elongation min. %

460

570-720

17

Previous:Shipbuilding Steel Plate EH32 Next:LR Grade AH32 DH32 EH32 FH32 steel